ALD (Atomic Layer Deposition) Ultratech Savannah-Thermal
Type: Deposition-CVD
Description: Deposit thin film one layer at a time using cycles of alternating precursors. Deposition rates vary depending on film and temperature but generally are about 1 Å per cycle.
Films: alumina (Al2O3), hafnium oxide (HfO2), silicon dioxide (SiO2), zinc oxide (ZnO), titanium dioxide (TiO2), and zirconium dioxide (ZrO2).
Substrate Compatibility: Varying sizes allowed, from pieces, all the way up to 6 inch wafers.